NASA Licenses 3D-Printable High-Temperature Superalloy That Can Last 2,500x Longer

NASA Superalloy GRX-810

NASA superalloy GRX-810 will soon be available to aviation and space industry parts manufacturers as a result of new licensing agreements with four U.S. companies. Credit: NASA/Jef Janis

<span class="glossaryLink" aria-describedby="tt" data-cmtooltip="

NASA
Established in 1958, the National Aeronautics and Space Administration (NASA) is an independent agency of the United States Federal Government that succeeded the National Advisory Committee for Aeronautics (NACA). It is responsible for the civilian space program, as well as aeronautics and aerospace research. Its vision is &quot;To discover and expand knowledge for the benefit of humanity.&quot; Its core values are &quot;safety, integrity, teamwork, excellence, and inclusion.&quot; NASA conducts research, develops technology and launches missions to explore and study Earth, the solar system, and the universe beyond. It also works to advance the state of knowledge in a wide range of scientific fields, including Earth and space science, planetary science, astrophysics, and heliophysics, and it collaborates with private companies and international partners to achieve its goals.

” data-gt-translate-attributes=”[{"attribute":"data-cmtooltip", "format":"html"}]” tabindex=”0″ role=”link”>NASA’s superalloy GRX-810, designed for extreme air and spaceflight conditions, is now being licensed to four American companies, enhancing the U.S. economy through improved aerospace components. This 3D-printable material increases the durability of parts, withstands severe temperatures, and promotes more sustainable aviation and space exploration.

NASA’s investment in a breakthrough superalloy developed for the extreme temperatures and harsh conditions of air and spaceflight is on the threshold of paying commercial dividends.

The agency is licensing its invention, dubbed “GRX-810,” to four American companies, a practice that benefits the United States economy as a return on investment of taxpayer dollars.

GRX-810 is a 3D-printable high-temperature material that will lead to stronger, more durable airplane and spacecraft parts that can withstand more punishment before reaching their breaking point.

The co-exclusive license agreements will allow the companies to produce and market GRX-810 to airplane and rocket equipment manufacturers as well as the entire supply chain.

The four co-exclusive licensees are:

  • Carpenter Technology Corporation of Reading, Pennsylvania
  • Elementum 3D, Inc. of Erie, Colorado
  • Linde Advanced Material Technologies, Inc. of Indianapolis
  • Powder Alloy Corporation of Loveland, Ohio

GRX-810 is one example of many new technologies NASA’s Technology Transfer Program managers review and file for patent protection. The team also works with inventors to find partners interested in commercialization. 

“NASA invests tax dollars into research that demonstrates direct benefit to the U.S. and transfers its technologies to industry by licensing its patents,” said Amy Hiltabidel, licensing manager at NASA’s Glenn Research Center in Cleveland.

3D Printed Turbine Engine Combusto

This turbine engine combustor (fuel-air mixer) was 3D-printed at NASA Glenn and is one example of a challenging component that can benefit from applying the new GRX-810 alloys. Credit: NASA

New Approach to Developing Materials

NASA engineers designed GRX-810 for aerospace applications, including liquid rocket engine injectors, combustors, turbines, and hot-section components capable of enduring temperatures over 2,000 degrees <span class="glossaryLink" aria-describedby="tt" data-cmtooltip="

Fahrenheit
The Fahrenheit scale is a temperature scale, named after the German physicist Daniel Gabriel Fahrenheit and based on one he proposed in 1724. In the Fahrenheit temperature scale, the freezing point of water freezes is 32 °F and water boils at 212 °F, a 180 °F separation, as defined at sea level and standard atmospheric pressure.&nbsp;

” data-gt-translate-attributes=”[{"attribute":"data-cmtooltip", "format":"html"}]” tabindex=”0″ role=”link”>Fahrenheit.

“GRX-810 represents a new <span class="glossaryLink" aria-describedby="tt" data-cmtooltip="

alloy
A mixture of two metallic elements typically used to give greater strength or higher resistance to corrosion.

” data-gt-translate-attributes=”[{"attribute":"data-cmtooltip", "format":"html"}]” tabindex=”0″ role=”link”>alloy design space and manufacturing technique that was impossible a few years ago,” said Dr. Tim Smith, materials researcher at NASA Glenn.

Smith co-invented the superalloy along with his Glenn colleague Christopher Kantzos using a time-saving computer modeling and laser 3D-printing process that fuses metals together, layer-by-layer. Tiny particles containing oxygen atoms spread throughout the alloy enhance its strength.

Impacts and Benefits

Compared to other nickel-base alloys, GRX-810 can endure higher temperatures and stress and can last up to 2,500 times longer. It’s also nearly four times better at flexing before breaking and twice as resistant to oxidation damage.

“Adoption of this alloy will lead to more sustainable aviation and space exploration,” said Dale Hopkins, deputy project manager of NASA’s Transformational Tools and Technologies project. “This is because jet engine and rocket components made from GRX-810 will lower operating costs by lasting longer and improving overall fuel efficiency.”

Research and development teams include those from Glenn, NASA’s Ames Research Center in California’s Silicon Valley, The Ohio State University, and NASA’s Marshall Space Flight Center in Huntsville, Alabama, where the most recent testing included 3D-printed rocket engine parts.

NASA develops many technologies to solve the challenges of space exploration, advance the understanding of our home planet, and improve air transportation. Through patent licensing and other mechanisms, NASA has spun off more than 2,000 technologies for companies to develop into products and solutions supporting the American economy.